Laboratory 3D Graphene Foam Material 



Introduction

The 3D Graphene Foam is made via chemical vapor deposition (CVD) processing. In course of CVD fabrication of graphene hydrogen and methane gases are introduced into a furnace that heats to 1000° Celsius. In the furnace is a nickel or copper film which captures a mono or multi-layer or graphene as the furnace is heated and the methane decomposes.


Advantages

1. It has good conductivity and is an excellent light porous conductive carrier.

2. On this substrate, we can grow a variety of oxide and hydroxide nanoarrays such as nickel oxide, cobalt oxide, cobalt trioxide, ferric oxide, cobalt hydroxide, nickel hydroxide, tungsten oxide, vanadium oxide, titanium oxide and so on.

 

Specifications

Sample size

100*100mm  can be customized)

Thickness

1.2 mm-1.6mm

Density

4 mg/cm3

Pore Size

580 microns

Packing

 in sealed membrane box 

Surface density
0.5-0.9 mg/cm2.
Size of branches
50-200 microns
Characteristic of  large aperture
200-500 microns.
Thermal conductivity
>6w/(m2k)
Standard PPI value
110

f

Dimensions

0.1mm*200mm*300mm

0.2mm*200mm*300mm

0.3mm*200mm*300mm

0.4mm*200mm*300mm

0.5mm*200mm*300mm

0.6mm*200mm*300mm

0.7mm*200mm*300mm

0.8mm*200mm*300mm

0.9mm*200mm*300mm

1mm*200mm*300mm

1.6mm*20mm*300mm

The size can be customized


To customize various metal foams, please click the picture below for details



Graphene Foam

graphene foam


graphene foam


graphene foam






related products

Copyright © Cheap Copper Foam, Iron Nickel Foam, Titanium Foam All Rights Reserved. Powered by dyyseo.com